I can't remember if it was here that someone
posted their method of treating cpm3v or not.
It involved a programable furnance because it
started:
1550 for 20min
ramp@2500 to 1990 and hold for 30min.
then it was press quenched on mag table
If whoever posted this could help I would
appreciate it. either here or e-mail me.
thanks
Gos

------------------
http://www.imt.net/~goshawk
Don't walk in tradition just because it feels good!!!!!
Romans 10:9,10
Hebrews 4:12-16
Psalm 91

 
Ed Schott heat treats CPM 3V but I don't know how to get in touch with him other than snail mail.