Hey Edward R Schott about your heat treat

Joined
Oct 4, 1998
Messages
418
Hey Edward do remember me I bought some Cpm3v from you? Well you said you could heat treat for me. How long a piece can you do? I am going to make a sword out of it. The piece is 36" and I want to use it all.

Also what kind of heat treatment do you use if you don't mind me asking?

------------------
-Greg Johnson
ICQ#4236341

 
yikes!!!!! three feet....even bill holt cant do a piece that long.....i think paul bos' limit is 22 inches.....
 
Well if can't do it I will build a temp controlled forge and do it myself.
smile.gif


------------------
-Greg Johnson
ICQ#4236341


 