Vanadis 8 SUPERCLEAN?

navman

Knifemaker / Craftsman / Service Provider
Joined
Mar 4, 2013
Messages
2,717
Does anyone have information (beyond what is on BUCORP's web site) or experience with VANADIS 8?

C 2.3
Si .4
Mn .4
Cr 4.8
Mo 3.6
V 8.0

64-65 HRC retaining toughness.
 
Do as much as You can before HT. After that it will be looooong run to grind anything. ;)

Definitely Agree! I use a lot of CPM S110V and do all my finish work pre-HT (I take the finish to 2000-2500 grit then back it down to level of finish I want post-HT)
 
Back
Top