AEB-L & CPM 3V, same heat treat?

Joined
Jun 11, 2006
Messages
8,651
I'm going to be sending out 4 3V blades for heat treating and wondering if I can toss in some AEB-L blades to offset the cost. I was looking at the heat treat specs and thy seam similar except it looks like 3V wants to soak for 30min where AEB-L 5Min. Thank you guys.
 
Peters did a batch like that for me a while back. They count knives that can go into the austenizing/quench oven together as a single batch. The temper at different temps, obviously.
 