- Joined
- Dec 23, 2008
- Messages
- 566
I'm working on my first camper slipjoint and I am wondering about tempering the bottle opener the same as the blades or possibly more? Anybody have any recomendations?
I am using O-1 tempering the blades at 375 degrees for one hour X 2.
I am using O-1 tempering the blades at 375 degrees for one hour X 2.
Last edited: