who does the heat treat for the production blades for fiddleback forge. And what is the Rockwell for s35vn? Looking at a production bushfinger, but no Rockwell hardness is listed.
I can first hand say the steel and HT are freaking awesome. I had a very hard spot when batoning a 2x4, got stuck and kept going. it literally bent a piece of the middle edge out close to 1/8" and was 1/4" tall. I lightly hammered it back straight on the vise anvil, stone it and you can't even tell it happend. Thats good stuff.
Thank you, I went ahead and ordered one from KSF. They seem to be a little scarece and aren't listed on the FF website anymore. Have had my eye on one for awhile.
Thank you, I went ahead and ordered one from KSF. They seem to be a little scarece and aren't listed on the FF website anymore. Have had my eye on one for awhile.