Has anyone heat treated using ITC 213 instead of Stainless pouch?

Joined
Feb 4, 2015
Messages
1
I have a friend who treats his knives with ITC 213 ceramic powder (mixed with water) painted onto the knives. He then heat treats by hanging them in kiln. Takes them out to air quench. Has anyone else tried this?
 