This should be asked in the Shop Talk section. I did find info on the Sandvik[ the maker] website but it took some time. www.smt.sandvik.com/strip Typical of the stainless steels it's hardened from 1975F for 5 min. Oil quench. Cryo treatment adds about 2 HRc. Temper about 400F