Normalizing/stress relieving 15N20

Joined
Oct 27, 2010
Messages
8,721
I have a piece I'm working on with .070" 15N20 and I put a radius bend in cold. Nothing drastic enough to cause fractures or anything, but I don't want to lose the specific radius in heat treat. What's a good schedule I could follow for stress relieving it before I finish grinding to prepare for HT? Should I just do a triple quench from 1450 down and the last one being sub-critical?