I have a few questions regarding my first parang. It is 1/4" 1084 and flat ground so far. I'm thinking of finishing it convexed. Should I take it to a zero gring on the edge or put a secondary bevel on it. If a secondary bevel how thick should I leave the edge? Where should the balance point be? I was going to temper at 450 degrees, should I go higher? Thanks
I have a few questions regarding my first parang. It is 1/4" 1084 and flat ground so far. I'm thinking of finishing it convexed. Should I take it to a zero gring on the edge or put a secondary bevel on it. If a secondary bevel how thick should I leave the edge? Where should the balance point be? I was going to temper at 450 degrees, should I go higher? Thanks