What happened to 3v versus sr-101?

Status
Not open for further replies.
I think someone here mailed someone else something. Testing would take a bit. Writing stuff is hard too. Give er time.
 
I look forward to Jerry's test results, especially regarding edge stability (any chipping?) of 3V. Corrosion resistance is also important to me - that is just one reason I choose INFI.
 
Last edited:
Don't hold your breath. Independent testers will give you a better idea of how it does.
 
Cobalt,

I look forward to the results from gsx-rboy750 as well. I am also interested to see how SR-101 does. Thank you both for contributing blades for this testing, and the time it takes! :thumbup:
 
I look forward to Jerry's test results, especially regarding edge stability (any chipping?) of 3V. Corrosion resistance is also important to me - that is just one reason I choose INFI.

there is no need to "test" Corrosion resistance on 3v and sr101, cause SR101 does not have corrosion resistance , just have 1% Cr.
 
there is no need to "test" Corrosion resistance on 3v and sr101, cause SR101 does not have corrosion resistance , just have 1% Cr.

I am pretty sure SR101 has 5% chrome. SR101, isn't exactly 52100, it is modified 52100
 
Is everything well with the test?

Well it has been 6 weeks and I have not heard a peep from him. Will have to pm him and see. I would assume that by now he has done something.
 