After a hiatus of several years, I'm trying to get back into the swing of things with a few unfinished projects. Here is the first:

Ux8yzUa.jpg

Cdaj8qT.jpg

gt2iUAj.jpg
 
Idk where everyone gets their WS gflex but it seems so expensive. Found a website that had these for under 20 bucks. But man they ship fast. From the time I ordered until the time it hit my front door was under 24 hours. Crazy. Wish combat Abbrassives shipped this fast. I ordered like 3 or 4 days ago and a ship ping label was just created today.
ObtU6Ww.jpg

Where'dja get it for under 20 bucks?
 
220 grit. I'm thinking about taking up to 800 before I heat treat. Then start back at 220 and finish with 400 and a soft backing. Depends how much hell this damn plunge give me. :mad::poop:
OCjykPo.jpg

Is,there a specific reason why you want to go to 800 pre-HT? Seems like that would be wasted effort.
 